MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici Radilon® A RV500HHR 3800 BK Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: PA66 50% glass fiber filled, injection molding grade with enhanced thermal resistance in contact with hot air. High improvement of mechanical properties retention versus standard polyamide 66 after heat aging. Black color. Alternative to special high temperature polymers in automotive applications like turbo air ducts, CAC tanks, EGR housing. High stiffness and mechanical resistance.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³DAM; ISO 1183
Moisture Absorption 1.20 %
@Thickness 2.00 mm,
Temperature 23.0 °C
1.20 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 210 MPa30500 psi5mm / min. DAM; ISO 527-2/1A
Elongation at Break 3.0 %3.0 %5 mm / min. DAM; ISO 527-2/1A
Tensile Modulus 15.9 GPa2310 ksi1mm / min. DAM; ISO 527-2/1A
Flexural Strength 340 MPa49300 psi2mm / min. DAM; ISO 178
Flexural Modulus 14.9 GPa2160 ksi2mm / min. DAM; ISO 178
Charpy Impact Unnotched  10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 11.0 J/cm²
@Temperature -30.0 °C
52.3 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.60 J/cm²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 1.70 J/cm²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cm1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohm1.00e+12 ohmDAM; 500V.; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 210 °C410 °FContinuous use
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75/2Af
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6929 / 293434

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.