Description: UNITHENE® LH503 is a high density polyethylene resin (HDPE) for use in injection and extrusion molding. Characteristics: - Good environmental stress cracking resistance
- Excellent stiffness
- High impact strength
Main Application: - Mineral water caps
- Sports knee and elbow pads
- Pallets
Information provided by USI Corporation |