MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Ketjenblack EC-600JD Processing Electroconductive carbon black
Categories: Other Engineering Material

Material Notes: Ketjenblack EC-600JD is a pure electroconductive carbon black extremely suitable for antistatic and electroconductive applications.

CAS number: 1333-86-4

EINECS/ELINCS No: 215-609-9

Applications: Ketjenblack EC-600JD is a very pure carbon black extremely suitable for antistatic and electroconductive applications. Due to its unique morphology and the extremely high surface area of approx. 1400 m2/g (BET), only one sixth the amount of Ketjenblack EC600-JD is needed compared to conventional electroconductive blacks in order to achieve the same conductivity. The extreme low loading of Ketjenblack EC600-JD allows easier processing for those compounds sensitive to filler addition, thus minimizing loss in mechanical and rheological properties. Ketjenblack EC-600JD when thoroughly dispersed with the polymer significantly increases the conductivity of the resulting compound. Ketjenblack EC-600JD can be used in all types of polymers, thermoset, thermoplastic as well as elastomers. Due to its unique morphology and structure with very low amounts of Ketjenblack EC-600JD excellent conductive material can be made. The loading needed to obtain a certain conductivity can vary significantly per type of polymer. More detailed information is available in the special Ketjenblack EC Technical Bulletin. Ketjenblack EC-600JD has a low ash content, which in addition with the extreme low loading level, makes it an excellent product for semicon applications in cable shielding. The low grit content provides very smooth surface during extrusion. Ketjenblack EC-600JD can also be used to produce conductive coatings and primers. Also here already at very low loading levels optimal electroconductive performance is obtained, which even more minimizes loss in mechanical and rheological properties compared to Ketjenblack EC-300J. With Ketjenblack EC- 300J about double the amount is needed to obtain the same conductivity Some other applications are batteries, packaging for IC parts, tubing, flooring, carpet backing, automotive parts, cell phones and many more.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.100 - 0.120 g/cc0.00361 - 0.00434 lb/in³
Volatiles <= 1.0 %<= 1.0 %
Particle Size <= 125 µm<= 125 µm= 7%, Fines
pH 9.0 - 10.59.0 - 10.5
Ash <= 0.10 %<= 0.10 %
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %
 
Descriptive Properties
AppearanceBlack free-flowing pellets
Content= 30 mg/kgGrit content
 1000-1100 mg/gIodine absorption
 480-510 ml/100gPore volume, DBP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY596 / 286119

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.