MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® 4000 CF20 Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: VESTAKEEP® 4000 CF20 is a carbon fiber reinforced (20%) polyether ether ketone for injection molding. The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 CF20 are self-extinguishing. VESTAKEEP® 4000 CF20 can be processed by common injection molding machines for thermoplastics. VESTAKEEP® 4000 CF20 is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners. Pigmentation may affect values.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Moisture Absorption 0.0300 %ISO 15512
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cmISO 294-4, 2577
Melt Flow 42 g/10 min
@Load 21.6 kg,
Temperature 400 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPaISO 527
Elongation at Break 2.5 %ISO 527
Tensile Modulus 16900 MPaISO 527
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 400 °C
Mold Temperature 160 - 200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting
Overview of materials for Polysulfone (PSU)
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Nylon 6, Unreinforced, Flame Retardant

PEVONIK810 / 243019

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.