MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® 2332 Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: LORD Chemlok® 2332 adhesive is a covercoat adhesive used to bond a wide variety of unvulcanized or vulcanized rubber compounds to Chemlok 205 and Chemosil® 211 primed metals or other rigid substrates. It is composed of a mixture of polymers, organic compounds and mineral fillers dissolved or dispersed in an organic solvent system. Chemlok 2332 adhesive will bond treated textiles to rubber during vulcanization process, and also bond compounds based on natural rubber (NR), polyisoprene (IR), styrene-butadiene (SBR), polybutadiene (BR), polychloroprene (CR), nitrile (NBR), hydrogenated nitrile (HNBR), butyl (IIR), millable polyurethane and polyepichlorohydrin (ECO) polymers to Chemlok 205 and Chemosil 211 primed metals and other rigid substrates.

Features: when used in combination with Chemlok 205 or Chemosil 211 primer, bonds a wide variety of cured and uncured elastomer compounds to rigid substrates; bonds treated textiles to rubber during vulcanization. resists hard settling. withstands temperatures, up to 149°C (300°F), often encountered during routine service of bonded assembly. provides rubber tearing bonds and excellent resistance to salt spray, heat and water when used in combination with Chemlok primer. applies easily by spray, dip, brush or roll coat methods.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.70 - 8.20 lb/gal
Solids Content 23 - 26 %by weight
Brookfield Viscosity 100 - 300 cP
@Temperature 25.0 °C
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 27.0 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 9.00 Month
@Temperature <=25.0 °C
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlack liquid
SolventsXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9015 / 232404

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.