MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials Vydyne® 67R NT0753 PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Vydyne 67R NT0753 is a high-viscosity, heat stabilized, PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. 67R NT0753 resin offers high strength, rigidity and toughness over a broad range of demanding applications and good fluid resistance to a wide variety of chemicals, solvents and oils.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DAM; ISO 1183
Water Absorption 1.8 %
@Time 86400 sec
1.8 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 2.4 %2.4 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.024 cm/cm
@Thickness 2.00 mm
0.024 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.024 cm/cm
@Thickness 2.00 mm
0.024 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 54.0 MPa7830 psi50% RH; ISO 527-2
 83.0 MPa12000 psiDAM; ISO 527-2
Elongation at Break 71 %71 %DAM; ISO 527-2
 97 %97 %50% RH; ISO 527-2
Tensile Modulus 1.40 GPa203 ksi50% RH; ISO 527-2
 2.90 GPa421 ksiDAM; ISO 527-2
Flexural Strength 30.0 MPa4350 psi50% RH; ISO 178
 90.0 MPa13100 psiDAM; ISO 178
Flexural Modulus 1.10 GPa160 ksi50% RH; ISO 178
 3.00 GPa435 ksiDAM; ISO 178
Poissons Ratio 0.380.38ISO 527-2
Izod Impact, Notched (ISO)  4.10 kJ/m²
@Temperature -30.0 °C
1.95 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 4.50 kJ/m²
@Temperature -40.0 °C
2.14 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 5.00 kJ/m²
@Temperature -40.0 °C
2.38 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 6.20 kJ/m²
@Temperature -30.0 °C
2.95 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 7.70 kJ/m²
@Temperature 23.0 °C
3.66 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.410 J/cm²
@Temperature -30.0 °C
1.95 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.450 J/cm²
@Temperature -40.0 °C
2.14 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.490 J/cm²
@Temperature -40.0 °C
2.33 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.570 J/cm²
@Temperature -30.0 °C
2.71 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  1.40e+11 ohm-cm
@Thickness 1.00 mm
1.40e+11 ohm-cm
@Thickness 0.0394 in
50% RH; IEC 60093
 2.70e+15 ohm-cm
@Thickness 1.00 mm
2.70e+15 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 71.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
39.4 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 76.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
42.2 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 262 °C504 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 184 °C363 °FUnannealed; 50% RH; ISO 75-2/B
 188 °C370 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FUnannealed; DAM; ISO 75-2/A
 94.0 °C201 °FUnannealed; 50% RH; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Middle Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Front Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Nozzle Temperature 280 - 310 °C536 - 590 °FInjection
Zone 1 250 - 295 °C482 - 563 °FExtrusion
Zone 2 250 - 295 °C482 - 563 °FExtrusion
Zone 3 250 - 295 °C482 - 563 °FExtrusion
Zone 4 250 - 295 °C482 - 563 °FExtrusion
Zone 5 250 - 295 °C482 - 563 °FExtrusion
Die Temperature 270 - 295 °C518 - 563 °FExtrusion
Melt Temperature 270 - 295 °C518 - 563 °FExtrusion
 285 - 305 °C545 - 581 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 60.0 - 75.0 °C140 - 167 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
Agency RatingsASTM, D4066
 ASTM, D6779
 EC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
 FDA, 21 CFR 177.1500
 RoHS Compliant
AppearanceNatural Color
Automotive Material SpecificationHMC MS 211-40
FeaturesChemical Resistant
 Gasoline Resistant
 General Purpose
 Good Toughness
 High Melt Stability
 High Rigidity
 High Strength
 High Viscosity
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodOther Extrusion
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9245 / 287598

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.