MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Leaded High-Strength Yellow Brass, UNS C86400, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Shrinkage in Solidification, Drossing; Medium – Fluidity; Low – Casting Yield, Effect of Section Size, Gassing

Fabrication Properties: Fair Suitability – Soldering, Brazing; Poor Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding

Typical uses: Door hardware for Prison; Window Hardware; Musical Instruments; Piano Keys; Electrical Components; Electrical Equipment; Switches; Screw Down Nuts; Bearing Cage Blanks; Bearings; Bushings; Cams; Fittings; Lever Arms; Light Duty Gears; Machinery Parts; Propellers; Pump Fixtures; Roller Bearings; Valve Stems; Boat Parts; Covers for Marine Hardware; Marine Fittings; Marine Hardware; Fixtures

Applicable Specifications: As Centrifugal Cast - Castings ASTM B271/B271M; As Sand Cast – Castings ASTM B584, ASTM B763/B763M; Ingot - ASTM B30, FEDERAL QQ-C-523

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.301 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 90
@Load 500 kg
 105
@Load 3000 kg
Tensile Strength >= 60.0 ksifor Standard
 65.0 ksiTypical
Tensile Strength, Yield >= 20.0 ksifor Standard, 0.5% Ext
 25.0 ksiTypical, 0.5% Ext
Elongation at Break >= 15 %for Standard
 20 %Typical
Tensile Modulus 14000 ksi
Compressive Strength 22.0 ksi0.001 in. set/in.
 87.0 ksi0.1 in. set/in.
Fatigue Strength 25000 psi
@# of Cycles 1.00e+8
Machinability 65 %
Izod Impact 30.0 ft-lb
Charpy Impact 25.0 ft-lbV-Notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000910 ohm-cm19% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 51.0 BTU-in/hr-ft²-°F
Melting Point 1583 - 1616 °F
Solidus 1583 °F
Liquidus 1616 °F
Shrinkage 2.08 %Patternmaker's Shrinkage (4/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 500 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.50 - 1.5 %
Copper, Cu 56 - 62 %
Iron, Fe 0.40 - 2.0 %
Lead, Pb 0.50 - 1.5 %
Manganese, Mn 0.10 - 1.5 %
Nickel, Ni <= 1.0 %
Tin, Sn 0.50 - 1.5 %
Zinc, Zn 34 - 42 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC86400x2 / 293169

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.