MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP39MAOHT Two component, thermally conductive, electrically insulative epoxy resin
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes:
  • Convenient handling
  • Low exotherm; well suited for large castings and potting
  • Withstands thermal cycling and shock
  • Good flow properties
Master Bond EP39MAOHT is a two component, thermally conductive, electrically insulative epoxy for bonding, sealing, coating, potting and encapsulation. The mix ratio is a forgiving one to one by weight, and after mixing, the epoxy flows smoothly. Upon mixing, this lower viscosity system has a relatively long working life. EP39MAOHT will cure at room temperature in 3-5 days. An alternative is to heat cure for 3-4 hours at 150-200°F. An optimum cure schedule would be overnight at room temperature followed by 3-5 hours at 150-200°F. EP39MAOHT has very low shrinkage and good dimensional stability upon curing. This epoxy is an excellent adhesive and bonds well to a wide variety of substrates including metals, ceramics, composites and glass as well as many rubber and plastic materials. An interesting aspect of EP39MAOHT is its ability to withstand rigorous thermal cycling, vibration and shock. EP39MAOHT is a good thermal conductor while retaining superior electrical insulation properties. This, combined with its good flow properties and lower exotherm, allows it to be used for potting and encapsulation applications of relatively larger sizes. It has reasonably good chemical resistance to water, fuels and hydraulics as well as many acids and bases. The service temperature range is -100°F to +400°F. The color of Parts A and Part B is off-white. EP39MAOHT might be used in aerospace, electronic, electrical, optical and specialty OEM applications.

Product Advantages:

  • Easy to use, non-critical one to one mix ratio by weight
  • Low viscosity, flows evenly and smoothly
  • Reliable thermal conductivity and electrical insulation
  • Low shrinkage and excellent dimensional stability
  • Resists thermal cycling, vibration and shock
  • Passes fungus resistance MIL-STD-810G

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 500 - 2000 cPPart B
 3000 - 6000 cPmixed
 30000 - 60000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80 - 90
Tensile Strength 4000 - 6000 psi
Tensile Modulus 400000 - 450000 psi
Compressive Strength 20000 - 22000 psi
Adhesive Bond Strength 1400 - 1600 psilap shear, Al/Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.8
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.30 - 1.44 W/m-K
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 4.00 hour
@Temperature 65.6 - 93.3 °C
 72.0 - 120 hour
@Temperature 23.9 °C
Working Life 120 - 150 minAfter mixing, 100 g batch
Shelf Life 6.00 MonthIn original unopened containers
 
Descriptive Properties
Cure scheduleovernight at 75°F plus 3-5 hours at 150-200°FOptimum
Mixing Ratio1:1Parts A to B, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP42HT-2AO Two Component, Thermally Conductive, Heat Resistant Epoxy
Master Bond LED401 White One Component LED Curable Adhesive System
Master Bond EP30AN Thermally Conductive Dimensionally Stable Epoxy System
Master Bond EP21TDC-2AO Flexibilized, Thermally Conductive Two Component Epoxy
Master Bond EP21TDC-2AN Two Component, Flexibilized, Highly Thermally Conductive, Electrically Insulating Epoxy Resin

PMASTM715 / 233772

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.