The resin DA076A is a high density polyethylene specially developed to manufacture film bioriented by tenter frame process. BOPE made with this resin has excellent stiffness and very stable run. Applications: Flexible packaging., Coextrusion of biaxially oriented film. Processes: BOPP film.Information provided by Braskem. |