MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Danquinsa DANPOL® PES-910 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: DANPOL PES-910 is a saturated, linear, medium crystalline copolyester in form of granules. DANPOL PES-910 is an optimal adhesive raw material for the application as hot-melt or solved in organic solvents. DANPOL PES 910 can also be excellent processed as a hot-melt adhesive granule by melt tank or extrusion process. From DANPOL PES-910 it could be also produced hot melt powders.

Application: The copolyester DANPOL PES-910 is used as a laminating adhesive. For this the granule DANPOL PES-910 can be dissolved in solvent. Also the melt-extrusion coating is possible. DANPOL PES-910 is well suited for the bonding of metallic materials with plastic, such as polyolefin films (PE and PP). Also the bonding of PET films with aluminum films is a typical application. Adhesives produced with DANPOL PES-910 also have good adhesion to ABS, polyester and polyamide textiles.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccDIN 53.479
Brookfield Viscosity 70000 - 80000 cP
@Temperature 160 °C
Thermosel, Melting
Melt Flow 125 g/10 min
@Temperature 160 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 3.0[mg KOH/g]
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 700 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 83.0 - 95.0 °CKofler
Softening Point 92.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 secRecrystallisation
 10.0 - 13.0 secOpen time
Shelf Life 6.00 Month
 
Descriptive Properties
AspectGranules
Hydroxyl value3-9 mg KOH/g
TypeSaturated, linear copolyester

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ165 / 294585

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.