LORD Thermoset P-1291 primer is designed for use in electronics applications to bond tin-catalyzed Room Temperature Vulcanized (RTV) silicone rubbers to most metals and glass. It may also be used to bond addition-cure silicones. Thermoset P-1291 primer is flammable (-8.33°C flash point). Do not store or use near heat, sparks or open flame. Features: provides good adhesion on most surfaces when using condensation-cure silicones, as well as addition-cure silicones. provides superior hydrolytic stability. All information provided by Lord. |