MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECACOMP PEEK 450 CMF white 1014868 Polyetheretherketone, Ceramic Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes:

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.870 g/cc0.0314 lb/in³EN ISO 60
Density 1.63 g/cc0.0589 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 100 MPa14500 psi50 mm/min; DIN EN ISO 527-1
Elongation at Break 12 %12 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 5.00 GPa725 ksi50 mm/min; DIN EN ISO 527-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.71e+15 ohm-cm2.71e+15 ohm-cmDIN EN ISO 3915
Surface Resistance 3.53e+15 ohm3.53e+15 ohmDIN EN ISO 3915
Dielectric Constant  4.76
@Frequency 1e+10 Hz
4.76
@Frequency 1e+10 Hz
DIN 53 481
 4.88
@Frequency 2.00e+9 Hz
4.88
@Frequency 2.00e+9 Hz
DIN 53 481
 4.89
@Frequency 1e+9 Hz
4.89
@Frequency 1e+9 Hz
DIN 53 481
 4.98
@Frequency 4.00e+9 Hz
4.98
@Frequency 4.00e+9 Hz
DIN 53 481
 5.01
@Frequency 3.00e+9 Hz
5.01
@Frequency 3.00e+9 Hz
DIN 53 481
 5.09
@Frequency 5.00e+9 Hz
5.09
@Frequency 5.00e+9 Hz
DIN 53 481
Dielectric Strength 15.8 kV/mm401 kV/inISO 60243-1
Dissipation Factor  0.00281
@Frequency 4.00e+9 Hz
0.00281
@Frequency 4.00e+9 Hz
DIN 53 481
 0.00287
@Frequency 3.00e+9 Hz
0.00287
@Frequency 3.00e+9 Hz
DIN 53 481
 0.0029
@Frequency 5.00e+9 Hz
0.0029
@Frequency 5.00e+9 Hz
DIN 53 481
 0.0039
@Frequency 2.00e+9 Hz
0.0039
@Frequency 2.00e+9 Hz
DIN 53 481
 0.0041
@Frequency 1e+9 Hz
0.0041
@Frequency 1e+9 Hz
DIN 53 481
Comparative Tracking Index 175 V175 VDIN EN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °FDIN 53765
Maximum Service Temperature, Air 260 °C500 °Flong term
 300 °C572 °Fshort term
Glass Transition Temp, Tg 143 °C289 °FDIN 53765
 
Processing PropertiesMetricEnglishComments
Processing Temperature 360 - 400 °C680 - 752 °FCylinder
Melt Temperature 390 - 400 °C734 - 752 °FMaterial temperature
Mold Temperature 160 - 210 °C320 - 410 °F
Drying Temperature 140 - 160 °C284 - 320 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9062 / 318990

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.