MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chengdu Letain PA6100 Blending (Alloy) Material
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Technical features: High stiffness and replacement of PA66; High-heat resistance; Parts of automobile and Parts of machines

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³GB1033
Water Absorption 1.3 %1.3 %GB1034
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 100 MPa14500 psiGB1040
Elongation at Break 10 %10 %GB1040
Flexural Strength 160 MPa23200 psiGB9341
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²GB1043
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmGB1410
Surface Resistance 1.00e+13 ohm1.00e+13 ohmGB1410
Dielectric Constant 4.0
@Frequency 1000 Hz
4.0
@Frequency 1000 Hz
GB1409
Dielectric Strength 30.0 kV/mm762 kV/inGB1408
Dielectric Loss Index 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
GB1409
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 220 °C428 °FGB1634
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGLT005 / 255858

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.