MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Arkema OREVAC® 18334 Grafted Maleic Anhydride Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene

Material Notes: OREVAC 18334 is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier bottle. OREVAC 18334 is mainly used in multi-layer bottle and tank to have good adhesion between PEHD, PA and EVOH. OREVAC 18334 combined with SOARNOL® from NIPPON GOSHEI provides very good oxygen barrier. These structures are used in milky products conditionings, fuel tanks and also industrial applications.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/cc
@Temperature 23.0 °C
ISO 1183
Melt Index of Compound 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 45ISO 868
Tensile Strength at Break 30.0 MPaASTM D638
Tensile Strength, Yield 4.50 MPaASTM D638
Elongation at Break 760 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 °CDSC
Vicat Softening Point 95.0 °C
@Load 0.999 kg
ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema OREVAC® 18510 Grafted Maleic Anhydride Polyethylene
Arkema OREVAC® 18380 Maleic Anhydride Modified Polyethylene
Arkema OREVAC® 18350 Grafted Maleic Anhydride Polyethylene
Arkema OREVAC® 18319 Grafted Maleic Anhydride Polyethylene
Arkema OREVAC® 18365 Maleic Anhydride Modified Polyethylene

PARKG117 / 80109

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.