MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Omnia Plastica Omniamid PA 6 - Akulon 6 - at 50% RH
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. The use of a high viscosity polymer for the extrusion of Akulon 6 stock shapes results in a product with excellent mechanical properties and a very high standard of quality.

Features:

  • Abrasion resistance: even in dusty and demanding environments, it’s one of the best engineering plastics.
  • Toughness: high tensile stress and compressive strength. The shock resistance is good particularly for annealed material.
  • Fatigue-proof: it maintains its features even under continuous stress.
  • Self-lubricating: the friction coefficient is low and generally for sliding applications it does not require lubricators.
  • Ageing resistance and weatherproof.
  • Natural colour.
Weak Point:

It is hygroscopic; it absorbs moisture which means that in time both its mechanical features and dimensions will change. When dry, it is hard and fragile and when moist it becomes more shock resistant and yielding. Machining is easy but automatic lathes should be avoided as the swarf is extremely elastic.

Application:

  • Mechanical: thanks to its features and its low price it is a popular material for "general purposes". Widely used in the mechanical industry to produce gears, cams, pulleys, anti-wear guides and other mechanical parts. It is used also for guides, bearings and wheels in shipbuilding. For outdoor applications, Akulon GX is preferable due to its higher UV stability.
  • Food contact: generally it is not used in contact with food.
  • Electrical: usage in the electrical field is to be avoided as the electrical features change with the moisture content.
  • Chemical : it is resistant to inorganic compounds and solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO.1183 DIN.53479
Moisture Absorption at Equilibrium 2.8 %50% relative humidity (beginning dry)
Water Absorption at Saturation 9.0 %23°C (beginning dry)
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 80.0 MPaISO2039.1 DIN.53456
Tensile Strength at Break 54.0 MPaISO.527 DIN.53455
Elongation at Break 180 %ISO.527 DIN.53455
Tensile Modulus 1.70 GPaISO.527 DIN.53455
Compressive Strength 6.00 MPa1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NB7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 2.50 J/cm²ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.42on dry ground steel; load =0.05MPa; speed =0.6 m/s (dry sample)
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 7.0
@Frequency 1e+6 Hz
ISO.250 DIN.53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
dry sample
Thermal Conductivity 0.250 W/m-KDIN.52612 (dry sample)
Melting Point 220 °C
Maximum Service Temperature, Air 88.0 °CContinuous; 5000 hours based on a tensile stress of 50% at 23° C. (dry sample)
 150 °Cshort period, no load (dry sample)
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °CISO.75 DIN.53461 (dry sample)
Minimum Service Temperature, Air -40.0 °Cimpact conditions and heavy loads not considered (dry sample)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celanex® 6500 PBT, 30% Mineral / Glass Reinforced
DSM Akulon® K-FHG0 (Dry) 50% Glass Reinforced Nylon 6 (North America)
DSM Akulon® K-FHG0 (Cond.) 50% Glass Reinforced Nylon 6 (North America)

POMNIA03 / 55604

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.