MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) KetaSpire® XT-920 CF30 PEEK, 30% carbon fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: KetaSpire® XT-920 CF30 is a 30% carbon fiber reinforced grade of the industry's first true a high-temperature PEEK. This compound provides the maximum level of mechanical properties at temperatures approaching 300°C. It also exhibits the lowest coefficient of linear thermal expansion (CLTE) within the KetaSpire® XT product family.

The PEEK designation is based on the 2:1 ratio of ether-to-ketone functional groups in the polymer backbone. The material provides the exceptional chemical resistance of PEEK along with a 20°C (36°F) higher glass transition temperature and a 45°C (81°F) higher melting temperature than standard PEEK. This increase in thermal performance allows engineers to achieve higher mechanical strength for components used in higher temperature and higher pressure operating environments.

Although other high-temperature polyketones exhibit thermal properties on par with KetaSpire® XT, their chemical resistance is significantly inferior to standard PEEK and KetaSpire® XT. The material's unique combination of properties makes KetaSpire® XT well-suited for applications in oil and gas, transportation, electronics, chemical processing, and other industrial uses.

Applications: Aircraft Applications; Automotive Applications; Connectors; Electrical/Electronic Applications; Gears; Industrial Applications; Oil/Gas Applications; Pump Parts; Thrust Washer

Features: Chemical Resistant; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Strength; Radiotranslucent; Steam Resistant

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccASTM D792
Viscosity 820 cP
@Shear Rate 1000 1/s,
Temperature 420 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow <= 0.0030 cm/cm
@Thickness 2.00 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 2.00 mm
ASTM D955
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 420 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 106ASTM D785
Hardness, Shore D 89
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 248 MPaASTM D638
 262 MPaType 1A; ISO 527-2
Elongation at Break 1.8 %Type 1A, 5 mm/min; ISO 527-2
 1.9 %5.0 mm/min; ASTM D638
Tensile Modulus 26300 MPa5.0 mm/min; ASTM D638
 26400 MPa1 mm/min, Type 1A; ISO 527-2
Flexural Strength 364 MPaASTM D790
 367 MPaISO 178
Flexural Modulus 22800 MPaISO 178
 23200 MPaASTM D790
Compressive Strength 190 MPaASTM D695
Shear Strength 107 MPaASTM D732
Izod Impact, Notched 93.0 J/mASTM D256
Izod Impact, Unnotched 830 J/mASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 51.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 4.10 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Melting Point 385 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 340 °CAnnealed; ASTM D648
Glass Transition Temp, Tg 170 °CDSC
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 405 °C
Middle Barrel Temperature 405 °C
Front Barrel Temperature 410 °C
Nozzle Temperature 410 °C
Mold Temperature 205 - 230 °C
Drying Temperature 150 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorBlack
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4352 / 280152

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.