MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Udel® P-1700 PSU, Transparent
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Transparent, general purpose for injection molding

Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged exposure to high temperatures and repeated sterilization. Udel® P-1700 polysulfone is highly resistant to mineral acids, alkali and salt solutions. Resistance to detergents and hydrocarbon oils is good, but the resin may be attacked by polar solvents such as ketones, chlorinated hydrocarbons and aromatic hydrocarbons.

These resins are also highly resistant to degradation by gamma or electron beam radiation. Electrical properties of Udel® P-1700 polysulfones are stable over a wide temperature range and after immersion in water or exposure to high humidity.

The resins comply with FDA 21 CFR 177.1655 and may be used in articles intended for repeated use in contact with foods. Additionally, they are approved by the NSF, by the Department of Agriculture for contact with meat and poultry and by the 3-A Sanitary Standards of the Dairy Association.

- Transparent: Udel® P-1700 CL 2611 CMP
- Transparent: Udel® P-1700 NT 06
- Transparent: Udel® P-1700 NT 11
- Opaque Black : Udel® P-1700 BK 937
- Opaque White: Udel® P-1700 WH 6417
- Opaque White: Udel® P-1700 WH 7407
- Opaque Gray: Udel® P-1700 GY 8057

Applications: Appliance Components; Appliances; Automotive Electronics; Dental Applications; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Hospital Goods; Industrial Parts; Medical Devices; Medical/Healthcare Applications; Microwave Cookware; Piping; Plumbing Parts; Surgical Instruments; Valves/Valve Parts

Features: Acid Resistant; Alcohol Resistant; Alkali Resistant; Autoclave Sterilizable; Biocompatible; Chemical Resistant; Detergent Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Food Contact Acceptable; Good Dimensional Stability; Good Sterilizability; Good Surface Finish; Good Toughness; Heat Sterilizable; High Heat Resistance; Hydrocarbon Resistant; Hydrolytically Stable; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cmASTM D955
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 343 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 70.3 MPaASTM D638
Elongation at Break 50 - 100 %ASTM D638
Tensile Modulus 2480 MPaASTM D638
Flexural Strength 106 MPaASTM D790
Flexural Modulus 2690 MPaASTM D790
Izod Impact, Notched 69.0 J/mASTM D256
Tensile Impact Strength 420 kJ/m²ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+16 ohm-cmASTM D257
Dielectric Constant 3.02
@Frequency 1e+6 Hz
ASTM D150
 3.03
@Frequency 60 Hz
ASTM D150
 3.04
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
Dissipation Factor 0.00070
@Frequency 60 Hz
ASTM D150
 0.0010
@Frequency 1000 Hz
ASTM D150
 0.0060
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 174 °CUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
 V-0
@Thickness 4.50 mm
Glow Wire Ignition Temperature 850 °C
@Thickness 1.60 - 6.00 mm
IEC 60695-2-13
 875 °C
@Thickness 0.800 mm
IEC 60695-2-13
Glow Wire Flammability Index 850 °C
@Thickness 0.800 mm
IEC 60695-2-12
 960 °C
@Thickness 1.60 - 6.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 329 - 385 °CInjection
Mold Temperature 121 - 163 °C
Drying Temperature 135 - 163 °C
@Time 12600 sec
Shot Size 50 - 75 %
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 177.1655
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorColors Available; Transparent - Slight Yellow
FormsPellets
ProcessingExtrusion; Extrusion Blow Molding; Film Extrusion; Injection Blow Molding; Injection Molding
 Machining; Pipe Extrusion; Profile Extrusion; Sheet Extrusion; Thermoforming
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4578 / 280378

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.