Hostacom PPT X9127 T 3143 is an unfilled polypropylene copolymer, with high impact resistance and good UV resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 3143 color version. This product is also available in other colors, new colors can be developed depending on customer requirements. Applications: Interior TrimsInformation provided by LyondellBasell. |