MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECACOMP PPA LDS black 1014979 Polyphthalamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes:
  • developed for the LPKF-LDS® process
  • high adhesive strength
  • good heat deflection temperature
Target Industries:
  • automotive industry
  • electrical engineering
  • LED lighting technology
  • mechanical engineering
former material REZ-RS-4108

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.96 g/cc
Water Absorption 0.35 %DIN EN ISO 1110
Linear Mold Shrinkage, Flow 0.0167 cm/cmDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0145 cm/cmDIN EN ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 76.0 MPaDIN EN ISO 527-1
Elongation at Break 1.2 %DIN EN ISO 527-1
Modulus of Elasticity 9.20 GPaDIN EN ISO 527-1
Charpy Impact Unnotched 25.0 kJ/m²DIN EN ISO 179-1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmDIN EN 61340-2-3
Surface Resistance 1.00e+15 ohmDIN EN 61340-2-3
Dielectric Constant 4.1
@Frequency 1e+9 Hz
Dissipation Factor 0.013
@Frequency 1e+9 Hz
Comparative Tracking Index 550 VDIN EN 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 43.0 µm/m-°C
@Temperature 50.0 - 100 °C
DIN EN ISO 11359-1;2
 62.0 µm/m-°C
@Temperature 100 - 150 °C
DIN EN ISO 11359-1;2
 97.0 µm/m-°C
@Temperature 150 - 200 °C
DIN EN ISO 11359-1;2
CTE, linear, Transverse to Flow 47.0 µm/m-°C
@Temperature 50.0 - 100 °C
DIN EN ISO 11359-1;2
 71.0 µm/m-°C
@Temperature 100 - 150 °C
DIN EN ISO 11359-1;2
 112 µm/m-°C
@Temperature 150 - 200 °C
DIN EN ISO 11359-1;2
Thermal Conductivity 0.900 W/m-Kin-plane; ISO 22007-4:2008
 1.20 W/m-Kthrough-plane; ISO 22007-4:2008
Melting Point 315 °C
Maximum Service Temperature, Air 150 °Clong term
 250 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 237 °CISO-R 75 Method A
Glass Transition Temp, Tg 120 °C
Flammability, UL94 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 300 - 340 °C
Mold Temperature 90.0 - 160 °C
Drying Temperature 120 °C
Dry Time 4.00 - 8.00 hour
Moisture Content <= 0.050 %Permissible residual moisture content
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIO9121 / 319049

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.