MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Jilin Xingyun Chemical XY-626 Antioxidant
Categories: Other Engineering Material

Material Notes: This product is soluble in benzene, chloroform, cyclohexane and other organic solvents, but insoluble in water, cold alcohol, and slight soluble in esters. This product is of low toxicity with good thermal stability and extraction of water-resistance, being effective in decomposing the hydrogen peroxide generated during thermal polymerization of process. As a new generation of high-temperature-type antioxidant, this product shows an excellent performance of thermal stability and color protection with good light stability under the condition of high temperature (above 300?), finding a wide application in polyolefin (PE , PP), PBT, PET, polypropylene fiber spinning, which undergo high-temperature processing and need high color protection under repeated high-temperature extrusion processing of plastic products with good performance. The product can also be used as light-resistant stabilizer such as synergist for benzophenone and benzotriazole.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %
@Temperature 80.0 °C,
Time 7200 sec
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 1.0[mgKOH/g]
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 170 °C
 
Descriptive Properties
AppearanceWhite crystalline powder
Content<2%Alkyl phenol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJILINX030 / 317877

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.