Product Description: A hard, colorable SEBS based thermoplastic elastomer (TPE) compound that offers good physical properties and chemical resistance. Bondable to: PP, EVA, PE Availability: Africa & Middle East; Asia Pacific; Europe; North America Features: Block Copolymer; Bondability; Good Colorability; Chemical Resistant; High Hardness RoHS Compliance: RoHS Compliant Appearance: Natural Color Forms: Pellets Processing Method: Injection MoldingInformation provided by Elastron |