MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Westlake EC808AA Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: WESTLAKE low-density polyethylene EC808 is a general-purpose formulation used for injection molding, general-purpose extrusion coating and laminating. It can be drawn down to low coating weights, is processable at high speeds, has a good moisture barrier, and is heat-sealable at low temperatures.

    Application/Uses
  • Foil
  • Food packaging
  • Laminating
  • Playing cards
  • Toys/sporting goods

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Can be drawn down to low coating weights, is processable at high speeds, has a good moisture barrier, and is heat-sealable at low temperatures
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/ccASTM D1505
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10.0 MPa500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 400 %500mm/min; ASTM D638 Type IV Specimen
2% Secant Modulus 207 MPa12.7mm/min; ASTM D790
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 - 330 °F
 
Descriptive Properties
ProcessCoating
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake EF412 Low Density Polyethylene
Arkema OREVAC® CA 100 Grafted Maleic Anhydride Polypropylene
Phillips 66 COPYLENE® CH350 Polypropylene Homopolymer
Westlake EC474AA Low Density Polyethylene
Westlake EM808AA Low Density Polyethylene

PWESF043 / 84480

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.