PROTEQ™ 7008 is an impact modified polypropylene compound. This grade has been formulated to retain a high resistance to impact at low temperatures combined with good rigidity. The grade is also stabilized to withstand intermittent exposure to UV radiation.Information provided by Ixom Operations PTY LTD |