Water clear, rigid polyurethane Key Properties: - Excellent physical properties
- Free of mercury, MOCA or TDI
- Low viscosity for excellent flow rates
Applications: - For room temperature hand-batch or vacuum assisted casting methods
- Applications with thin wall sections
Cure 1: 24 hours at 77°F + 16 hours at 180°F Cure 2: 7 days at 77°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |