MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Celanese Ateva® 1850A Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Ateva® 1850A resin is suitable for use in hot melt coating and adhesive applications, it is also well suited for use in compounds and masterbatch applications. It contains an antioxidant to minimize viscosity changes of the hot melt blends during processing. It complies with Code of Federal Regulation 21 CFR Section 177.1350 and 175.105, subject to extraction limitations for specific end use applications. This polymer may be processed on conventional extrusion equipment. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Additives: Antioxidant

Applications: Adhesives & Sealants; Compounds & Masterbatches

Information provided by Celanese Corporation.

Key Words: hot melt coating and adhesive applications; well suited for use in compounds and masterbatch applications
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.937 g/ccASTM D1505; ASTM D1928 Proc A
Vinyl Acetate Content 18 %AT Plastics PTM-39
Melt Flow 150 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 86ASTM D2240
Hardness, Shore D 37ASTM D2240
Tensile Strength at Break 8.00 MPaType IV (50 mm/min); ASTM D638
Elongation at Break 700 %Type IV (50 mm/min); ASTM D638
Flexural Modulus, 1% Secant 0.0360 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 49.0 °CASTM D1525
Brittleness Temperature -40.0 °CASTM D746
Ring & Ball Softening Point 95.0 °CASTM E28
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Ateva® 1608 EVA polymer for compounds, molding and tubing
Celanese Ateva® 2604A Ethylene Vinyl Acetate Copolymer
Celanese Ateva® 1820 Ethylene Vinyl Acetate Copolymer
Celanese Ateva® 1615 Ethylene Vinyl Acetate Copolymer Coating Resin
Celanese Ateva® 1211A EVA polymer for flexible packaging

PATEVB04 / 25960

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.