MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Trinseo MAGNUM™ 575 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Product Description: MAGNUM™ 575 is a medium heat, high stiffness, and very high impact resistant ABS that is suitable for extrusion and thermoforming applications. This material is available in North America
Benefits: Lot to lot consistency for optimal machine parameters; Self-coloring improvement to lower costs in pigments and logistics; Low VOC to improve interior air quality; Heat stability for processing temperatures to improve part design; Low gels for excellent thermoformablity with low levels of scrap
Applications: Recreational vehicles; Panels; Signs

Complies with: US FDA 21 CFR 181.32

Availability: North America

Features: Good Processability; High Toughness

Uses: Bathroom Accessories; Construction Applications; Consumer Applications

Agency Ratings: FDA 21 CFR 181.32

Form: Pellets

Processing Method: Injection Molding; Profile Extrusion; Sheet Extrusion; Thermoforming

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 294-4
Melt Flow 1.4 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 4.8 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 6090 psi2.0 in/min; ASTM D638
 6960 psiISO 527-2/50
Elongation at Break 15 %ISO 527-2/50
 17 %2.0 in/min; ASTM D638
Tensile Modulus 290000 psiIOS 527-1/1
 305000 psi0.039 in/min; ASTM D638
Flexural Modulus 363000 psi0.079 in/min; ISO 178
 377000 psi0.051 in/min; ASTM D790
Izod Impact, Notched 4.40 ft-lb/in
@Temperature -30.0 °C
ASTM D256
 9.60 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Charpy Impact, Notched 21.0 ft-lb/in²Injection Molded; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 147 °FUnannealed; ASTM D648
Vicat Softening Point 207 °FISO 306/B50
 
Processing PropertiesOriginal ValueComments
Drying Temperature 176 - 194 °F
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRINSE1539 / 312232

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.