Eastman Cristal™ Renew 401-99.9 copolyester is a high flow product that contains mold release for ease of ejection. It is designed and engineered specifically for cosmetics packaging applications. With its unsurpassed color and clarity and an unmatched ability to mold thick parts with improved gate aesthetics, Cristal™ 401-99.9 Renew is clearly a well-suited copolyester for premium cosmetics packaging. Other outstanding features of Cristal™ Renew 401-99.9 copolyester are excellent chemical resistance, high gloss, and improvements in processing such as faster cycle times, and lower scrap rates. Cristal™ Renew 401-99.9 is also ideally suited for two-shot molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow characteristics. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation. Applications - Bottles-color cosmetics pkg
- Color cosmetics packaging
- Jars-skin care pkg
- Personal care & cosmetics packaging
- Skin care packaging
Key Attributes- Ability to mold thick parts
- Ease of processing
- Easy to extrude, cut, decorate, and seal
- Excellent clarity and color
- Excellent colorability
- Good impact strength
- Good stiffness
- High gloss appearance
- Improved gate aesthetics
- Readily fill intricate molds
- Toughness
Information provided by Eastman. |