MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ 2410 PEI (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 40% Glass Fiber

Material Notes: 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.61 g/ccASTM D792
Water Absorption 0.13 %
@Time 86400 sec
ASTM D570
Moisture Absorption at Equilibrium 0.90 %ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 5.2 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 114ASTM D785
Tensile Strength at Break 179 MPaType I, 5 mm/min; ASTM D638
Tensile Strength, Yield 186 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 2.5 %Type I, 5 mm/min; ASTM D638
Flexural Strength 241 MPa2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 11720 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 112 J/mASTM D256
Izod Impact, Unnotched 427 J/mASTM D4812
Tangent Modulus 11720 MPa5 mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+16 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 0.00 - 100 VUL 746A
Hot Wire Ignition, HWI >= 120 secUL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.4 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 212 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 234 °CRate B/50; ASTM D1525
UL RTI, Electrical 170 °CUL 746B
UL RTI, Mechanical with Impact 170 °CUL 746B
UL RTI, Mechanical without Impact 170 °CUL 746B
Flammability, UL94 V-0
@Thickness 0.250 mm
UL 94
 5VA
@Thickness 1.47 mm
UL 94
 5VA
@Thickness 1.50 mm
UL 94
Smoke Density 1.0
@Time 240 sec
Flaming, Ds; ASTM E 662
Oxygen Index 54 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 1 330 - 400 °C
Zone 2 340 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °C
Mold Temperature 135 - 165 °C
Drying Temperature 150 °C
Dry Time 4.00 - 6.00 hour
 24.0 hourCumulative
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI22690 / 215826

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.