NORYL™ GFN1720 resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade was developed for high heat applications and exhibits a good balance of heat resistance, strrength, and electrical performance. NORYL GFN1720 resin is an excellent candidate for applications requirinng electrically insulating properties, such as ignition coils and bobbins.Information provided by SABIC |