MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Melos Mecoline IS RDX 1231 F Halogen-free, radiation cross-linkable, flame retardant compound
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, radiation cross-linkable, flame retardant compound

Compound class: Insulation / sheathing

Compound category: RDX

Flame retardant: ATH

Standards: EN 50264 EM 101, 102, 103 and 104

Typical applications: It is an excellent choice for single core power cable for protected, fixed installation inside and outside railway vehicles for connecting fixed parts in direct current and alternating voltage technology, especially converter technology. The Mecoline IS RDX 1231 F compound is very low temperature resistant to – 40°C and IRM 902 & IRM 903 oil resistant

Features: Flame retardant; Halogen-free; Low smoke; Oil resistant; High temperature resistant; Flexible; Flexible at low temperatures

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/cc
pH >= 4.5Corrosivity; IEC 60754-2
Melt Flow 7.0 g/10 min
@Load 21.6 kg,
Temperature 175 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85pressed plaques; DIN ISO 7619-1
Tensile Strength >= 9.00 MPaextruded tapes; IEC 60811-501
 >= 12.0 MPacross-linked plaques or tapes, 75kGy; IEC 60811-501
 <= 10.25 MPa
@Temperature 120 °C,
Time 864000 sec
cross-linked plaques / tapes, After ageing in air oven; IEC 60811-401
 <= 11.7 MPa
@Temperature 100 °C,
Time 259000 sec
cross-linked plaques / tapes, Fluid IRM 902; IEC 60811-404
 <= 11.7 MPa
@Temperature 70.0 °C,
Time 605000 sec
cross-linked plaques / tapes, Fluid IRM 903; IEC 60811-404
Elongation at Break >= 180 %cross-linked plaques or tapes, 75kGy; IEC 60811-501
 >= 200 %extruded tapes; IEC 60811-501
 24 %
@Temperature -60.0 °C
cross-linked plaques / tapes; IEC 60811-505
 >= 35 %
@Temperature -40.0 °C
cross-linked plaques / tapes; IEC 60811-505
 <= 10 %
@Temperature 200 °C,
Time 900 sec
Hot set test, Residual, 0.2 Mpa; IEC 60811-507
 <= 40 %
@Temperature 200 °C,
Time 900 sec
Hot set test, under load, 0.2 Mpa; IEC 60811-507
 <= 250 %
@Temperature 120 °C,
Time 864000 sec
cross-linked plaques / tapes, After ageing in air oven; IEC 60811-401
 <= 280 %
@Temperature 100 °C,
Time 259000 sec
cross-linked plaques / tapes, Fluid IRM 902; IEC 60811-404
 <= 280 %
@Temperature 70.0 °C,
Time 605000 sec
cross-linked plaques / tapes, Fluid IRM 903; IEC 60811-404
Penetration <= 50
@Temperature 140 °C,
Time 14400 sec
IEC 60811-508
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+10 ohm-cmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 170 °CTool
 170 °CMaximum mass temperature
Zone 1 130 - 140 °C
Zone 2 150 - 160 °C
Zone 3 160 - 170 °C
Zone 4 160 - 170 °C
Zone 5 160 - 170 °C
Adapter Temperature 160 - 170 °C
Head Temperature 160 - 170 °C
Drying Temperature 60.0 °C
Dry Time 4.00 hour
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 40 %ASTM D 2863 A
 
Descriptive Properties
Conductivity=4.0 µS/mmpressed plaques, IEC 60754-2
Main burning properties<540 mmBurning test (vertical), EN 60332-1-2
 0Halogen content, IEC 754-1
Shrinkage<2%1h at 120°C, IEC 60811-502
Temperature index300°CASTM D 2863 D
Toxicity index2EN 50305

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMELOS034 / 296141

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.