MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUCENE™ SP988 Metallocene Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Applications: Hot & cold drinking water pipe, Floor heating, Radiator connection, Al composite pipe

  • LUCENETM SP 988, LG PE-RT (Type?) is a high performance MDPE for hot and cold water pipe. It is developed by using a new LG catalyst technology.
  • It has excellent stress crack resistance properties and Long Term Hydrostatic strength.
  • LUCENETM SP 988 Polyethylene Resin meets requirements of the FDA regulation 177.1520 and NSF/ANSI Standard 61 (Drinking Water System Components - Health Effect).

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.941 g/ccASTM D1505
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ISO 868
Tensile Strength at Break >= 36.0 MPaASTM D638
Tensile Strength, Yield 204 kg(f)/cm²ASTM D638
Elongation at Break 750 %ASTM D638
Flexural Modulus 6730 kg(f)/cm²ISO 178
Izod Impact, Notched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 128 °C
Vicat Softening Point 125 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLHCHEM9914 / 239430

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.