MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® RF006EU PA66-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Vydyne RF006EU is an UV stabilized, 30% glass fiber reinforced PA66+PA6 for injection molded applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccDAM; ISO 1183
Water Absorption 3.0 %
@Time 86400 sec
DAM; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 170 MPaDAM; ISO 527-2
Elongation at Yield 3.3 %DAM; ISO 527-2
Tensile Modulus 8800 MPaDAM; ISO 527-2
Flexural Strength 233 MPaDAM; ISO 178
Flexural Modulus 7600 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Hot Wire Ignition, HWI 7.0 - 15 secPLC 4; UL 746
 7.0 - 15 secPLC 4; UL 746
High Amp Arc Ignition, HAI 60 - 120 arcsPLC 1; UL 746
 >= 120 arcsPLC 0; UL 746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 215 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 130 °C
@Thickness 1.50 mm
UL 746
 130 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 105 °C
@Thickness 1.50 mm
UL 746
 105 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 115 °C
@Thickness 1.50 mm
UL 746
 115 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 255 - 275 °CInjection
Middle Barrel Temperature 265 - 275 °CInjection
Front Barrel Temperature 265 - 275 °CInjection
Melt Temperature 265 - 275 °CInjection
Mold Temperature 70.0 - 90.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.20 %Injection
 
Descriptive Properties
Agency RatingsISO, 1043 PA66+PA6 GF30
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8539 / 296316

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.