MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Pressure Seal 21747 Polyacrylate
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 21747 is a 70 durometer black colored general purpose Polyacrylic polymer. It exhibits good resistance to compression set, heat and petroleum based oils. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 DF 712 A26 B16 B36 EO16 EO36; 5 DF 708 A26 B16 EO16 EO36; 3 DH 715 A26 B16 B36 EO16 EO36 F13; 5 DH 708 A26 B16 EO16 EO36 F13

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73
 65
@Temperature 150 °C,
Time 252000 sec
ASTM OIL #3
 74
@Temperature 150 °C,
Time 252000 sec
Service Fluid 100
 76
@Temperature 150 °C,
Time 252000 sec
ASTM OIL #1
 80
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 80
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
Tensile Strength 1760 psi
 56.3 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 56.3 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 1578.7 psi
@Temperature 150 °C,
Time 252000 sec
ASTM OIL #3
 1744.2 psi
@Temperature 150 °C,
Time 252000 sec
Service Fluid 100
 1867.4 psi
@Temperature 150 °C,
Time 252000 sec
ASTM OIL #1
Elongation, Ultimate 220 %
 159.9 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 159.9 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 190.08 %
@Temperature 150 °C,
Time 252000 sec
ASTM OIL #1
 190.1 %
@Temperature 150 °C,
Time 252000 sec
ASTM OIL #3
 210.9 %
@Temperature 150 °C,
Time 252000 sec
Service Fluid 100
100% Modulus 763 psi
Tear Strength 179 pliDie B
Compression Set 14.4 %
@Temperature 150 °C,
Time 79200 sec
Solid
 23.4 %
@Temperature 150 °C,
Time 252000 sec
Solid
 24.8 %
@Temperature 150 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature 14.0 °F
Shrinkage -0.400 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM OIL #1
 1.8 %
@Temperature 150 °C,
Time 252000 sec
Volume, Service Fluid 100
 12.4 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM OIL #3
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL249 / 318459

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.