MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ITW Spraycore® AlphaFill Lightweight Putty
Categories: Polymer; Thermoset

Material Notes: AlphaFill Lightweight is a high quality, tack-free, lightweight putty with excellent adhesion to metal, galvanized metal, aluminum, fiberglass and wood. BPO catalyst is not included. Product features: Smooth texture offers great spreading, excellent featheredge and clog free sanding properties, great adhesion to corrosion treated metals, formulated for low exothermic. Product benefits: incredible user friendly, metal preparation does not require coarse grinding, preserving the factory corrosion protection. Preferred red dye catalyst: BPO.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0420 lb/in³Application density
Viscosity 102000 - 120000 cP102000 - 120000 cPSSA W/T-E Bar @ 20 rpm
 
Chemical PropertiesMetricEnglishComments
Styrene Content 15 - 20 %15 - 20 %
 
Processing PropertiesMetricEnglishComments
Pot Life 3.00 - 5.00 min3.00 - 5.00 min
 
Descriptive Properties
ColorLight grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWS9050 / 239560

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.