MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Composiflex FlexPLY™ High Performance Composite Spring, Crossply 1:1
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: A variety of carbon/epoxy, E-glass epoxy, and high-temperature glass/epoxy springs and available for industrial equipment uses. Some examples of these types of machinery include conveyors, oscillating sanders, vibratory rollers, vibratory feeders, and more.

Crossply - Fibers alternate 0° and 90° at specified intervals, typically 1:1. Example 0,90,0,90,0,90,0.
Available thickness per ply: 0.005 in. and 0.010 in.

Mechanical property data measured on 0.15 in thick samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 67
Tensile Strength 62.9 ksi
@Temperature 71.1 °C
ASTM D3039
 70.2 ksi
@Temperature 22.8 °C
ASTM D3039
Tensile Modulus 4.39e+6 psi
@Temperature 71.1 °C
Chord Modulus from 0.1 to 0.3%, P; ASTM D3039
 4.70e+6 psi
@Temperature 22.8 °C
Chord Modulus from 0.1 to 0.3%, P; ASTM D3039
Flexural Strength 84.6 ksi
@Temperature 71.1 °C
ASTM D790
 92.3 ksi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 3210 ksi
@Temperature 71.1 °C
ASTM D790
 3470 ksi
@Temperature 22.8 °C
ASTM D790
Compressive Strength 50.6 ksi
@Temperature 71.1 °C
ASTM D3410
 67.6 ksi
@Temperature 22.8 °C
ASTM D3410
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.82
@Frequency 1e+6 Hz
50% RH; ASTM D150
 4.98
@Frequency 100000 Hz
50% RH; ASTM D150
 5.17
@Frequency 1000 Hz
50% RH; ASTM D150
 5.25
@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 428 kV/in50% RH; ASTM D149
Dissipation Factor 0.0070
@Frequency 60 Hz
50% RH; ASTM D150
 0.0080
@Frequency 1000 Hz
50% RH; ASTM D150
 0.018
@Frequency 100000 Hz
50% RH; ASTM D150
 0.038
@Frequency 1e+6 Hz
50% RH; ASTM D150
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 265 °FDMA, E'

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOMPOS92 / 282296

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.