MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chemours Krytox™ AUT 2C45 PFPE Automotive Performance Lubricant
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Krytox™ 2C grease is made using Krytox™ PTFE and a non-melting thickener. Anti-corrosion additive. Anti-wear additive. Extreme pressure additive.

These synthetic fluorinated lubricants are used in extreme conditions. They are nonflammable and safe for use in oxygen service. They are chemically inert and are used safely around hazardous chemicals. They do not damage plastics or elastomers or cause corrosion to metals. They are commonly used as lubricants in aerospace, automotive, industrial, and semiconductor applications, as well as solving many other routine lubrication problems.

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.00 g/cc
@Temperature 0.000 °C
Volatiles <= 0.20 %
@Treatment Temp. 66.0 °C,
Time 79200 sec
ASTM D2595
 <= 2.0 %
@Treatment Temp. 121 °C,
Time 79200 sec
ASTM D2595
Viscosity Measure 2.5 cSt
@Temperature 204 °C
base oil
 12.5 cSt
@Temperature 100 °C
base oil
 100 cSt
@Temperature 40.0 °C
base oil
 310 cSt
@Temperature 20.0 °C
base oil
 
Mechanical PropertiesOriginal ValueComments
Oil Separation 4.0 %
@Treatment Temp. 99.0 °C,
Time 108000 sec
wt% loss
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -44.0 °C
 
Descriptive Properties
AppearanceWhite, Creamy Consistency
Standard NLGI Grade2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDUPJ827 / 254015

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.