Compound 4751 is a black colored, high quality and sulfur free Neoprene W elastomer. It has a good balance of physical properties and good aging properties. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 3 BC 715 A14 B14 C12 EO14 EO34 F17 G21; 5 BC 715 A14 B14 C12 EO14 EO34 G21; 6 BC 715 A14 B14 C12 EO14 EO34 F17 G21; 2 BE 720 A14 B14 C12 EO14 EO34 F17; 3 BE 720 A14 B14 C12 EO14 EO34 G21 AMS 3209 AMS 3244 Information provided by Pressure Seals Inc. |