MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Entec Estane® 58246 TPU TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Product Description: Type: Estane® 58246 is a 50D aromatic Polyester-Based Thermoplastic Polyurethane (TPU)
Features: High stiffness grade with excellent chemical and oil resistance.
Uses: Flat Die/Cast Film Extrusion and Injection Molding

Availability: Asia Pacific; Latin America; North America

Features: Aromatic; Chemical Resistant; High Stiffness; Oil Resistant

Uses: Cast Film

Agency Ratings: FDA 21 CFR 177.1680; FDA 21 CFR 177.2600

RoSH Compliance: RoSH Compliant

Forms: Pellets

Processing Method: Cast Film; Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 47 - 53
@Time 5.00 sec
ASTM D2240
Tensile Strength at Break 9300 psi
@Thickness 0.762 mm
ASTM D412
Tensile Stress 1800 psi
@Strain 100 %,
Thickness 0.762 mm
ASTM D412
 4450 psi
@Strain 300 %,
Thickness 0.762 mm
ASTM D412
Elongation at Break 420 %
@Thickness 0.762 mm
ASTM D412
Tear Strength 180 pliSplit; ASTM D470
 801 pli
@Thickness 0.762 mm
Die C; ASTM D624
Tensile Set 12 %
@Strain 200 %
ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 320 °FKofler
 338 °F
Glass Transition Temp, Tg -40.0 °F
 
Processing PropertiesOriginal ValueComments
Zone 1 390 °F
Zone 2 399 °F
Zone 3 410 °F
Zone 4 421 °F
Adapter Temperature 430 °F
Die Temperature 430 °F
Melt Temperature 424 °F
Drying Temperature 219 °F
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENTB670 / 311363

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.