MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem Accelerator TMTD-OT powder
Categories: Other Engineering Material

Material Notes: Product Description: TMTD is a very active, sulfur-bearing, non-discoloring rubber accelerator for use in NR, SBR, NBR, EPDM as well as other rubber elastomers and blends. For most compounding applications, TMTD requires the addition of zinc oxide and fatty acid for effective use. Sulfur is not required but is often used. It is widely used as a primary accelerator for curing systems requiring very low or no sulfur. TMTD is often used to activate thiazole or sulfenamide cure systems. Accelerator TMTD is also available in a pellet form and micro granules (MG) to reduce dusting. TMTD contains 13% available sulfur. Improved scorch resistance can be obtained in TMTD stocks by the use of the thiazole or sulfenamide accelerators as a primary accelerators. TMTD is an off-white to light gray in color.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/cc
Ash 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 144 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH461 / 315379

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.