MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chesterton 615 HTG #1 Grease  (discontinued **)
Categories: Fluid; Lubricant

Material Notes: Description: Chesterton® 615 HTG #1 is the versatile performer needed in all applications requiring a heavy duty NLGI #1 grease. The outstanding extreme pressure characteristic of this grease, coupled with its excellent water washout resistance makes it a truly superior choice for tough applications. The corrosion protection provided to surfaces lubricated with 615 is far greater than virtually all competitive greases. Unlike many NLGI #1 greases, 615 will not bleed or age harden. It can be pumped through grease dispensing systems with ease permitting labor savings through automation. It is important when choosing a lubricant to select the lightest lubricant that will effectively reduce friction and wear between moving parts. An NLGI #1 grease becomes especially important at higher bearing speeds and/or in equipment subject to very low temperatures. This is because at very high speeds, a heavier grease will generate more drag or friction on the moving part than is desirable. At very low temperatures, a #2 grease. Under both of these conditions Chesterton 615 HTG #1 provides distinct and valuable benefits over currently available products.

Features:

  • Easily pumpable in automatic grease dispensing systems
  • Will not bleed or age harden
  • Exceptional shear and roll stability
  • Excellent protection against corrosion in high moisture environments
  • Superior choice for extremes of temperature and pressure
  • NSF H2 - Registration number 133941
  • ISO L-XCDIB1
  • DIN 51 502-KPF 2P-30

Applications: 615 HTG #1 should be used to lubricate parts and equipment in any industrial area subject to extreme pressure and severe conditions where a softer consistency grease is called for. It is especially effective when operating speeds are high or in cases where temperatures routinely fall below 0°C (32°F). Uses can be found in the following industries:Metal working:On machine tools, mechanical presses, milling heads, reduction gears, exposed gears, cams, toggle joints, links and other components.Pulp and Paper:On calendar bearings, high speed spindle gears, and most devices under load in humid or wet conditions where the grease's excellent water washout resistance and corrosion protection will protect lubricated partsSteel:On continuous casters, couplings, oscillators, torch pin rolls, automatic torches, shears, blowers and other uses where the grease's high temperature performance will reduce relubrication frequencyMining:On conveyers, grinding mills, crushers, hoists and bearings.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 70ASTM D2596, DIN 51 350/4
Four Ball Extreme Pressure, Weld Load 620 kgASTM D2596, DIN 51 350/4
Four Ball Wear 0.400 mmScar Diameter; ASTM D2266, DIN 51 350/5
Penetration 310 - 340ASTM D217, DIN ISO 2137
Oil Separation 0.20 %loss; ASTM D1742
Timken Test 60.0 lbOK Load; ASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -45.0 °C
Dropping Point 300 °CASTM D2265, DIN 51 801/1
 
Descriptive Properties
Bearing Life120 hoursASTM D3527
ColorBlue-Green
Consistency1NLGI, DIN 51 818
Corrosion Resistance>1000 hrs@ 50 microns film thickness, 5% NaCl, ASTM B117
Shear Stability+1.4%10000 strokes, ASTM D217
 +2.8%100000 strokes, ASTM D217
TextureButtery with slight tack
Water Washout Resistance<1.0%@ 79°C (175°F), ASTM D1264

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTCHS068 / 138180

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.