MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Zortrax Z-PEI 1010 Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Z-PEI 1010 is a blend of PEI slightly stronger than Z-PEI 9085 and with higher heat deflection temperature. The material can withstand temperatures reaching 208° C. It is also harder than Z-PEI 9085 which makes it perfect for scenarios where high rigidity is of paramount importance. Moreover, it offers broad chemical resistance to automotive fluids, fully halogenated hydrocarbons, alcohols, and aqueous solutions among others.

Applications:

  • components with high rigidity
  • temperature resistant parts
  • chemically resistant parts.

Information provided by Zortrax

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 56.0 MPaISO 527
Elongation at Break 3.0 %ISO 527
Tensile Modulus 2500 MPaISO 527
Flexural Strength 110 MPaISO 178
Flexural Modulus 2510 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 208 °CISO 75
Glass Transition Temp, Tg 217 °C
Flammability, UL94 HB
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZORT000 / 281879

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.