MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials Semitron® ESD CNT PEEK Polyetherether Ketone (ASTM Product Data Sheet)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Developmental product data sheet.

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc
@Temperature 22.8 °C
1.33 g/cc
@Temperature 73.0 °F
ASTM D792
Water Absorption 0.10 %0.10 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.58 %0.58 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 126126ASTM D785
Tensile Strength 110 MPa
@Temperature 22.8 °C
15900 psi
@Temperature 73.0 °F
ASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Tensile Modulus 4.34 GPa
@Temperature 22.8 °C
630 ksi
@Temperature 73.0 °F
ASTM D638
Flexural Strength 170.0 MPa
@Temperature 22.8 °C
24650 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus 4.16 GPa
@Temperature 22.8 °C
604 ksi
@Temperature 73.0 °F
ASTM D790
Compressive Strength 119 MPa
@Strain 10 %,
Temperature 22.8 °C
17300 psi
@Strain 10 %,
Temperature 73.0 °F
ASTM D695
Compressive Modulus 4.14 GPa
@Temperature 22.8 °C
600 ksi
@Temperature 73.0 °F
ASTM D695
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D256 Type A
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+6 - 1.00e+7 ohm1.00e+6 - 1.00e+7 ohmEOS/ESD S11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 48.6 µm/m-°C
@Temperature -40.0 - 149 °C
27.0 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Melting Point 340 °C644 °FASTM D3418
Maximum Service Temperature, Air 246 °C475 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Est Rating per resin data
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative YesYes
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ColorDark Gray/Black
Machinability71-10, 1=Easier to Machine

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SM1A_a / 265839

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.