MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Excelite Plastic AS-200 Anti-scratch polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Excelite Anti-scratch polycarbonate provides enhanced strength of abrasion and impact resistance. It is ideal where good visibility is of paramount importance and in applications where unwanted scratches are to be avoided. It is specially formulated to withstand contact from a wide range of cleaning agents and organic solvents. Anti-scratch polycarbonate sheet has an abrasion resistant coating;

These coatings provide the ultimate in:

  • Protection against scratching & abrasion
  • preventing chemical attack
  • optical clarity
  • outdoor weather protection
  • graffiti resistance
  • ease of cleaning
Potential Applications:
  • Auto industry
  • Electronic industry
  • Machine Accessories
  • Protective mask

Information provided by Excelite Plastic Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccGB/T 1003
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
GB/T 1033
Thickness 1500 - 12000 microns59.1 - 472 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.3 MPa8750 psiGB/T 1040
Elongation at Break >= 90 %>= 90 %GB/T 1040
 108 %108 %Tensile; GB/T 1040
Elongation at Yield 6.0 %6.0 %GB/T 1040
Modulus of Elasticity 0.240 GPa34.8 ksiGB/T 9341
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C35.0 µin/in-°FGB/T 1034
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Lucent PC-1428 Polycarbonate, Injection Grade
Covestro Makrolon® 2205 Polycarbonate, Injection Grade
Covestro Makroblend® UT250 HR PC+PET
Evonik TEGOMER® AntiScratch L Additive
Evonik TEGOMER® AntiScratch 200 Polyamide compound

PEXLT002 / 198712

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.