Compound 5716 is a 70 durometer black colored Buna N elastomer, it is formulated for low temperature flexibility. It exhibits good resistance to petroleum based oils and gasoline type fuels. It also offers good resistance to boiling water. The working temperature range for this compound is -40°F to 212°F with intermittent peaks to 250°F. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BF 715 B14 B34 EO14 EO34; 2 BG 715 B14 B34 EO14 EO34 EF11 EF21 EA14 F17; 5 BG 715 A14 B14 B34 EO14 EO34 This Compound is RoHS Compliant Information provided by Pressure Seals Inc. |