MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

ASI® RP 1500 Cyanoacrylate Super Glue
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: RP 1500 is a high viscosity, rapid curing, cyanoacrylate adhesive. It is designed to bond a wide range of similar and dissimilar materials. Handling strength in most applications is in 15 seconds.

Substrates bonded include ABS, Acrylic, Aluminum, Bakelite, Brass, Chloroprene, Chrome, Cooper, EPDM, Fiberglass, Latex, Leather, Natural Rubber, NBR, Neoprene, Nitrile, Nylon, Phenolic, Polycarbonate, Polyester, Polystyrene, Porcelain, PVC, SBR, Steel, Valox, and Wood.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/cc
Viscosity 1500 cP1500 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 12.4 MPa>= 1800 psivs. Steel; ISO 6922
Adhesive Bond Strength >= 5.17 MPa>= 750 psiNeoprene substrate. Fixture time < 5 sec; ISO 4587
 >= 5.86 MPa>= 850 psiPhenolic substrate. Fixture time < 10 sec; ISO 4587
 >= 6.21 MPa>= 900 psiABS substrate. Fixture time < 10 sec; ISO 4587
 >= 6.21 MPa>= 900 psiPVC substrate. Fixture time < 5 sec; ISO 4587
 >= 6.21 MPa>= 900 psiPolycarbonate substrate. Fixture time < 30 sec; ISO 4587
 >= 12.1 MPa>= 1750 psiAluminum substrate. Fixture time < 15 sec; ISO 4587
 >= 14.5 MPa>= 2100 psiSteel substrate. Fixture time <20 sec; ISO 4587
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 - 1.00e+16 ohm-cm2.00e+15 - 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.0 - 3.5
@Frequency 1000 Hz
2.0 - 3.5
@Frequency 1000 Hz
ASTM D150
Dissipation Factor <= 0.020
@Frequency 1000 Hz
<= 0.020
@Frequency 1000 Hz
ASTM D 150
 
Descriptive Properties
BaseEthyl
Color / appearanceclear
Strength Retained100%. Aged 500 hrs, Ethanol @22°C.
 100%. Aged 500 hrs, Freon TA @22°C.
 100%. Aged 500 hrs, gasoline @22°C.
 100%. Aged 500 hrs, isopropanol @22°C.
 100%. Aged 500 hrs, Motor oil @ 40°C.
 100%. Aged 500 hrs, Polycarbonate @ 40°C & 95% RH.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1005 Steel
304 Stainless Steel
Armacell Ensolite™ ECF-400 EPDM crushed foam
Aluminum, Al
Aluminum Spelling Note

PASINC9010 / 233377

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.