Advantages: - silencing, impact resistance flexibility, spring ability creep resistance, solvent resistance
- Excellent heat stability, the best heat stability in TPE
- Good bendable at low temperature, it bears cold to -54?
- Good mechanical strength
- Great bendability and fatigue resistance
- Crystallize quickly; shaping easily
- Oil and medicine resistance
- Low water absorbing rate, good size stability
- Good wear resistance, low frictional coefficient
Applications: - Wire inner skin
- Hydraulic tube
- Bended tube
- Telephone wire outer skin
Information provided by Go Yen Chemical |