MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Estane® MVT 80 NT1 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Polyether Thermoplastic Polyurethane (TPU)

Features: High Moisture Vapor Transmission, Oeko-Tex® Standard 100 Compliant

Uses: Extrusion: Film, Sheet, Fabric Coating

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccResin, 30 mil films; ASTM D-792
Water Vapor Transmission 1000 g/m²/day
@Thickness 0.0254 mm
Upright Cup; ASTM E-96 B
 4500 g/m²/day
@Thickness 0.0254 mm
A1; JIS L1099
 6000 g/m²/day
@Thickness 0.0254 mm
Mocon; ASTM D-6701
 12000 g/m²/day
@Thickness 0.0254 mm
Inverted Cup; ASTM E-96 BW
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80Resin, 30 mil films; ASTM D2240
Hardness, Shore D 31Resin, 30 mil films; ASTM D2240
Tensile Strength at Break 3500 psi
@Thickness 0.0254 mm
Film; ASTM D-882
Tensile Strength 27.6 MPaResin, 30 mil films; ASTM D-412
Elongation at Break 800 %Resin, 30 mil films; ASTM D-412
 420 %
@Thickness 0.0254 mm
Film; ASTM D-882
100% Modulus 4.10 MPa
@Strain 100 %
Resin, 30 mil films; ASTM D412/D638
 7.58 MPa
@Strain 100 %,
Thickness 0.0254 mm
Film; ASTM D-882
300% Modulus 6.90 MPa
@Strain 300 %
Resin, 30 mil films; ASTM D412/D638
 16.2 MPa
@Strain 300 %,
Thickness 0.0254 mm
Film; ASTM D-882
Tear Strength 16.6 kN/mSplit, Resin, 30 mil films; ASTM D-470
 68.3 kN/mResin, 30 mil films; ASTM D-624 Die C
 15.8 kN/m
@Thickness 0.0254 mm
Film, Average; ASTM D-1938
 <= 22.8 kN/m
@Thickness 0.0254 mm
Film; ASTM D-1938
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 °C
Glass Transition Temp, Tg 37.0 °C
 
Processing PropertiesOriginal ValueComments
Zone 1 166 - 177 °C
Zone 2 170 - 182 °C
Zone 3 177 - 188 °C
Zone 4 182 - 193 °C
Adapter Temperature 182 - 193 °C
Die Temperature 177 - 188 °CZone 2
 182 - 193 °CZone 1
Screw Speed 15 - 40 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR5024 / 238894

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.