MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Zortrax Z-PCABS Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Z-PCABS is a unique blend which combines the properties of two materials: ABS and polycarbonate (PC). Its advantages include high mechanical durability, and resistance to various factors, including high temperatures. Z-PCABS is perfectly suited for industrial use as it allows you to test your prototypes and end-use parts regardless of extreme conditions. You will benefit from this fusion of materials while creating housings of everyday tools, constructional elements of various equipment, and automotive components which will remain stable and fully functional over time.

Information provided by Zortrax

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.139 g/ccISO 1183-3:2003
Melt Flow 30.07 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133:2006
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73ISO 868:1998
Tensile Strength at Break 34.76 MPaISO 527:1998
Tensile Strength 36.89 MPaISO 527:1998
Elongation at Break 8.56 %ISO 527:1998
Elongation at Yield 6.93 %ISO 527:1998
Flexural Strength 58.4 MPaISO 178:2011
Flexural Modulus 1270 MPaISO 178:2011
Izod Impact, Notched (ISO) 11.4 kJ/m²ISO 180:2004
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 104.1 °CISO 11357-3:2014

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZORT007 / 281886

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.