Partially aromatic copolyamide with a combination of semi-crystalline polyamide reinforced with 45% glass fiber, heat stabilized and lubricated for injection molding process. Eplamid HT00 grades offer the following unique properties in general conditions, and even after moisture absorption: - Good surface finish
- Good dimensional stability
- Good high temperature properties
- Outstanding chemical resistance to glycols and oils
- Excellent creep resistance
Eplamid HT00 grades are used for molding technical parts where higher operating temperatures and higher stiffness in moist environments are required. Information provided by Epsan Plastik |