Poly(3-butylthiophene-2,5-diyl) (P3BT) is an alkylthiophene based conducting polymer that can be used as a donor molecule in the development of organic electronics. It is a p-conjugating polymer with a p-p stacking distance of 0.395 nm. Applications: P3BT can act as a hole transporting layer (HTL) which can potentially be used in the fabrication of organic field effect transistors (OFETs), chemical sensors, rechargeable batteries and polymeric solar cells (PSCs). Molecular Formula: C10H16S IUPAC Name: 3-butyl-2,5-dimethylthiophene Synonyms: P3BT SMILES: CCCCC1=C(SC(=C1)C)C InChI=1S/C10H16S/c1-4-5-6-10-7-8(2)11-9(10)3/h7H,4-6H2,1-3H3; InChiKey = DUOSBQJOYVIVOR-UHFFFAOYSA-N Alfa Chemistry Materials product group: Polymer/Macromolecule Manufacturer data sheet |
Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |